LINQCELL ANO-NiAl

Harmonization Code : 7508.10.00.00 | Cloth, grill and netting, of nickel wire

LINQCELL NWM-ANO

Main features

  • Low overpotential for oxygen evolution reaction
  • Platinum-group metal (PGM)-free catalyst
  • Optimized as anode for alkaline water electrolyzers

Product Description

LINQCELL ANO-NiAl is a nickel-based electrode with a binary nickel–aluminum alloy catalyst layer deposited through plasma spray coating. It exhibits low overpotential for the oxygen evolution reaction (OER), which is the anodic half-reaction in both hydrogen generation and CO2 conversion systems. Traditionally, precious metals, such as iridium and ruthenium are used as OER catalysts. However, nickel-based materials, such as the LINQCELL ANO-NiAl, are emerging as strong alternatives to platinum-group metals due to their high reaction rates and long-term stability. The binary alloy composition further improves catalytic performance and oxidation resistance.

Key Features:

  • High Catalytic Activity for OER: The nickel-based electrode, with its binary nickel-aluminum alloy catalyst layer, exhibits low overpotential for the oxygen evolution reaction (OER), a crucial reaction in both hydrogen generation and CO2 conversion.
  • Cost-Effective Alternative to Precious Metals: By utilizing nickel-based materials, ANO-NiAl significantly reduces the reliance on expensive precious, thus lowering capital expenditures.
  • Improved Performance and Stability: The binary alloy composition of the catalyst layer enhances both the catalytic performance (high reaction rates) and the oxidation resistance of the anode, contributing to long-term stability and efficient operation.

These feature make LINQCELL ANO-NiAl an ideal high-performance anode for both alkaline water electrolyzers and alkaline carbon dioxide electrolyzers.

Highly Recommended for:

LINQCELL ANO-NiAl comes in different sizes and different woven mesh & perforated sheets substrates to meet various device design requirements. Contact us for custom sizes or other specific requirements.

 

Product Family

ANO-NiAl/40X40S4019

400mm x 400mm | 4019 Wire Mesh Substrate
1. Select Sheet Size
2. Select Alloy Type

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Sheet
Net weight 0.1 kg
Gross weight 0.12 kg
Dimensions 40 x 40 x 0.5 cm
TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

LINQCELL ANO-NiAl Properties

Property Parameter Test Method / Conditions
Mechanical Stability Weight loss < 1% Ultrasonication / 120 W, 60 min
Electrochemical Stability Performance decay <2% Cyclic voltammetry/
–1.5 to –0.3 V vs. Hg/HgO (200 cycles) at 30% KOH, 30 (±1)°C

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers