Assembly Films

Conductive and Insulating

Assembly Film Adhesives

Assembly adhesives in film format are an increasing topic of interest. They have similar formulations to traditional die attach pastes and assembly pastes but they come in sheets with custom dimensions that can be applied directly on the die or substrate. These flat and even conductive and non conductive die attach films ensure perfect uniformity and a very controlled bond line thickness. Additionally, there’s minimal overflow during assembly and custom die-cut designs can also be produced.

Industry trends for electronic devices can be summarized as Miniaturization, High power dissipation, Higher reliability, Thinner devices. All these trends have certain drawbacks and challenges for die attach and assembly pastes. Miniaturiazation means that it is easier to contaminate the adjacent wirebond pads by flow and bleed from the adhesive. Higher reliability faces difficulties because of the difficult set-up and process maintenance that can lead to incomplete coverage, uneven fillet height, suck back, and other issues. In addition to that, the warpage of the die makes dies harder to stack, while contamination of the die surface from the adhesive is a possibility. Finally, thinner devices are prone to inconsistent fillets that can reduce reliability. The position accuracy is very important to avoid tilt while the contamination of the wire bonding pads by flow and bleed from the adhesive still lurks. All of the above problems can be resolved by assembly adhesives due to their controlled flow.

26 products

RecommendedPrice low to highPrice high to low
  • LOCTITE ABLESTIK 550K

    LOCTITE ABLESTIK 550K

    • Low cure temperature
    • Hard to bond metals
    • Thermally conductive
  • ABLESTIK 506

    ABLESTIK 506

    • Flexible Cured Adhesive
    • 0.9 W/(m K) Thermal Conductivity
    • Reworkable Bonding Material
  • ABLESTIK 550

    ABLESTIK 550

    • Film-Format Bonding for Difficult Surfaces
    • 30-Minute 150 deg C Cure
    • 39 N/mm^2 Aluminum Lap Shear
  • ABLESTIK 568

    ABLESTIK 568

    • 2.5 x 10^14 ohm-cm Volume Resistivity
    • 2-Hour 95 deg C Cure
    • 3 mil Glass-Fabric-Supported Film
  • ABLESTIK CF3366

    ABLESTIK CF3366

    • 0.0003 ohm-cm Volume Resistivity
    • 5.17 N/mm^2 Aluminum Lap Shear
    • Flexible Cured Adhesive
  • ABLESTIK ECF 550

    ABLESTIK ECF 550

    • Conductive Grounding and RF-Shielding Film
    • Controlled Film Processing with Flexible Supply Formats
    • 20 N/mm^2 Lap Shear
  • ABLESTIK ECF561E-1

    ABLESTIK ECF 561E

    • Electrically Conductive Bonding
    • Flexible Cured Adhesive
    • 1.6 W/(m K) Thermal Conductivity
  • ABLESTIK ECF 568

    ABLESTIK ECF 568

    • Electrically Conductive Application
    • 2-Hour 95 deg C Cure
    • Sheet Stock or Die-Cut Preforms
  • ABLESTIK 5074

    ABLESTIK 5074

    • Flexible Dissimilar-Material Bonding
    • Multiple Heat-Cure Options
    • Reworkable Non-Conductive Film
  • ABLESTIK 517-4-007/009

    ABLESTIK 517

    • Tack-Free Non-Conductive Film
    • 24-Hour Work Life at 25 deg C
    • 30-Minute 150 deg C Cure
  • ABLESTIK 539IA

    ABLESTIK 539IA

    • Polyester-Carrier Epoxy Film
    • 1-Month Work Life at 25 deg C
    • 1-Hour 150 deg C Cure
  • ABLESTIK ECF506

    ABLESTIK ECF506

    • Glass-Fabric Bondline Control
    • 24-Hour Work Life at 25 deg C
    • 125 deg C Thermal Rework

Product selector guide

Electrically Conductive Assembly FIlms
Product CVCM (%) TML (%) TC(W/mK) Resistivity (Ohms*cm) Glass transition temperature (°C) CTE a1 CTE a2 Recommended cure Attributes
LOCTITE ABLESTIK 5025E 0.06 0.3 6.5 5x10-4 90 65 150 30min @150°C Hot devices and PC on heatsinks. NASA
LOCTITE ABLESTIK CF3350 0.03 0.16 7 2x10-4 90 65 150 30min @150°C  PC, Backplanes, Heatsinks on fluoropolymer, ceramic, copper, kovar, Al
LOCTITE ABLESTIK ECF563 0.02 0.21 1 1x10-3 88 60 250 30min @150°C  RF/EMI shielding. Microwave substrate in packages
LOCTITE ABLESTIK ECF564A 0.01 0.3 2.2 4x10-4 150 30 - 2hours@150°C Ultra low outgassing. MIL
LOCTITE ABLESTIK ECF564AHF 0.01 0.3 3 4x10-4 122 80 330 2hours@150°C High flow version of 564A

 

Non Conductive Assembly FIlms
Product CVCM (%) TML (%) TC(W/mK) Resistivity (Ohms*cm) Glass transition temperature (°C) CTE a1 CTE a2 Recommended cure Attributes
LOCTITE ABLESTIK 5020 0.01  0.4  0.2   5x1014 100 60 200 1hour @150°C Substrate attach. Seal packages. NASA
LOCTITE ABLESTIK 5020K 0.02 0.24 0.7 8X1015 109 45 270 1hour @150°C Higher purity 5020
LOCTITE ABLESTIK 550K - - 0.8 7.2x1012 102 50 300 30min @150°C Heat sink bonding
LOCTITE ABLESTIK 561 - - 0.3 5x1012 50 85 300 30min @150°C For mismatched CTEs
LOCTITE ABLESTIK 561K - - 0.9 9.1X1012 55 85 300 30min @150°C Reworkable. NASA
LOCTITE ABLESTIK 563K 0.04 0.44 1.1 - 97 45 300 30min @150°C Hot devices on heatsinks
LOCTITE ABLESTIK 564A 0.01 0.3 0.3 2x1015 140 35 15 2hours @150°C High purity. Bond hybrid substrates
LOCTITE ABLESTIK 566K - - 0.8 1.4x1013 93 85 300 2hours @100°C Low temp cure
LOCTITE ABLESTIK 570K - - 0.7 6x1014 135 50 35 3hours @150°C High purity. Adhesion to Gold. Reliable

 

Optical Conductive Assembly FIlms
Product Adhesive Adhesive thickness
(µm)
Adhesion strength (Oz/in) Operating temperature
(°C)
Visible light transmission Attributes
ITO-125 - - - - >85% -
ITO-175 - - - - >85% -
OCA Acrylic 10 70 -40 ~ +110 >92% -

Frequently asked questions

How does environmental exposure affect Assembly films for RF grounding?


Optimization of the cure schedule showed that improved performance was achieved after the use of increased temperature during cure. Exposure to high-temperature storage was shown to provide more stable temperature dependant adhesion strength.

Generally, the films maintain relatively good levels of temperature-dependent adhesion strength after 250 hrs of high-temperature exposure over the range of temperatures tested. Prolonged moisture soak (85ºC/85%RH) exposure was shown to have a minor effect in regards to mechanical and electrical performance. This suggests that for applications requiring both good resistance to high temperatures and moisture-rich environments, films may offer good performance. Read more in this paper.

What are the benefits of assembly films?


With increasing functionality and power requirements for electronic equipment, the need for thermal management is critical. The demand for uniformed bondline application as well as the avoidance of air inclusions across large areas make epoxy film adhesives essential for many applications in the aerospace, telecommunications, and electronics fields. Luckily, assembly films not only provide best-in-class electrical, thermal, and mechanical performance, but also lower total assembly costs through the elimination of inventory maintenance and/or third-party conversion.

Assembly films provide a proven solution for the most demanding applications requiring the highest reliability performance. Henkel’s epoxy film adhesives are perfectly suited for large bonding areas that also require uniformed bondlines and custom sizes and shapes. For this reason, we provide customized film preforms to precisely match highly-complexhighly complex printed circuit board shapes and patterns. This ensures an exact amount of void-free adhesive with a controlled bondline thickness in a specific area. We offer heat activated film adhesives that help reduce curing time and increase the efficiency of your work processes.

 


Learn more

Assembly films for controlled flow

assembly films for controlled flow

Assembly films - Application notes and Handling guide

 

Henkel epoxy based film products are designed for use in a variety of PCB or hybrid applications. This includes such applications as basic heatsink attach, die attach, coining, and grounding for gigahertz frequency RF parts. All Henkel film products are prepared into a dry “B-staged” state where they can be easily handled with minimal need for tools or equipment. Products are available in three basic categories: Electrically Conductive, Thermally Enhanced, or Non-Filled films. Electrically Conductive Films: Conductive films are specially designed to maximize electrical conductivity while giving a variety of other options such as: low temperature cure, high flexibility, superior adhesion, and/or high thermal stability. LOCTITE® ABLESTIK CF 3350, the core product in this line, combines high conductivity and flexibility with superb adhesion and homogeneity to make it an excellent choice for most mid or high-end applications.

Electrically Conductive Films: Conductive films are specially designed to maximize electrical conductivity while giving a variety of other options such as: low temperature cure, high flexibility, superior adhesion, and/or high thermal stability. LOCTITE® ABLESTIK CF 3350, the core product in this line, combines high conductivity and flexibility with superb adhesion and homogeneity to make it an excellent choice for most mid or high-end applications. Thermally Enhanced Films: Henkel

Thermally Enhanced Film products offer the perfect blend of high thermal conductivity with varying degrees of flexibility and adhesion specially formulated for heatsinking or thermal dissipation applications.

Non-Filled Films: Non-Filled Film Products may be used for various applications including electrical isolation, liquid crystal displays, solvent resistant bonding, or basic substrate assembly.

 

Application Techniques

Substrates: Film products provide excellent adhesion to a large variety of substrate materials, including most metals, ceramics, and PWB materials.

Cutting and Custom Preforms: For most applications, the most convenient and cost-effective cutting solution is to obtain die cut preforms prepared directly from customer supplied CAD drawings. For prototype or low volume applications, cutting sheet stock with a razor blade or scissors may suffice. Tacky films may require that the release liner be left on for this step. For larger volume applications, selected products are available in reel format for in-situ cutting as part of the assembly process.

 

Cleaning & Handling: Product is ready to use upon removal of polyester or silicone paper release liners, and green plastic interleaf layers. While cleaning of substrates is not mandatory, an organic solvent wipe is recommended to remove any oils that might interfere with the bonding process or electrical interface. Plasma cleaning is also recommended, though it may enhance film flow. Substrates and film product may easily be assembled by hand as desired. While not required, the use of gloves is recommended to reduce the chance of contamination.

Storage & Handling: All film products have a recommended set of storage conditions. Check the Technical Data Sheet for conditions specific to each product. Most films recommend storage from - 40 to 0°C. It is best to leave sheets or preforms bagged until use. Thawing time varies depending on quantity of film removed, but may be as little as a few minutes for a single sheet. Once thawed, it is not recommended to restore back to the freezer.

Pre-Tacking: In some small area applications such as die attach, it may be desirable to pre-tack the substrates into place. Most products will develop a moderate amount of tack when heated to temperatures in the range of 40 – 60°C. After preheating one substrate to this temperature, the film may be gently applied and tacked into place by either sandwiching it between the release Liner and substrate, or between both substrates being attached*. From here, parts may be cooled to room temperature before exposing to the final cure profile. It is possible to cure very small parts without applied pressure if they are adequately pre-tacked.

Cleaning & Handling: Product is ready to use upon removal of polyester or silicone paper release liners, and green plastic interleaf layers. While cleaning of substrates is not mandatory, an organic solvent wipe is recommended to remove any oils that might interfere with the bonding process or electrical interface. Plasma cleaning is also recommended, though it may enhance film flow. Substrates and film product may easily be assembled by hand as desired. While not required, the use of gloves is recommended to reduce the chance of contamination.

Storage & Handling: All film products have a recommended set of storage conditions. Check the Technical Data Sheet for conditions specific to each product. Most films recommend storage from - 40 to 0°C. It is best to leave sheets or preforms bagged until use. Thawing time varies depending on quantity of film removed, but may be as little as a few minutes for a single sheet. Once thawed, it is not recommended to restore back to the freezer.

assembly films

Pre-Tacking: In some small area applications such as die attach, it may be desirable to pre-tack the substrates into place. Most products will develop a moderate amount of tack when heated to temperatures in the range of 40 – 60°C. After preheating one substrate to this temperature, the film may be gently applied and tacked into place by either sandwiching it between the release Liner and substrate, or between both substrates being attached*. From here, parts may be cooled to room temperature before exposing to the final cure profile. It is possible to cure very small parts without applied pressure if they are adequately pre-tacked.

 

Curing

Time & Temperature: All products have at least one recommended cure profile as listed on the Technical Data Sheet for that product. It is highly recommended to stay to these conditions as curing at different temperatures may cause the film to wet the substrate poorly, or possibly not fully cure. If a different cure temperature is needed, consult customer support for possible advice on this or consider an alternative product that will better fit the application. Most products list cure profiles at 150°C with an alternative cure at 125°C. It is also important to note that cure times are listed as a minimum temperature exposure at the bondline. Larger metal parts may take a significant amount of time to reach peak temperature and will therefore need longer to bond properly. Most products may be safely cured for times longer than needed with negligible adverse effects.

Cure Pressure: Adequate pressure is needed to ensure that the film fully wets substrate surfaces during the cure profile. The following chart gives recommended** cure pressures for most major products.

 

Troubleshooting

Pressure Application: Films need applied pressure during cure to promote proper wetting of substrate surfaces. Henkel recommends the use of spring clamps, lamination presses, or vacuum bagging to achieve even and predictable pressure during the cure process. No matter what method is used, it is important to evenly distribute pressure over the entire contact area to ensure even wetting and a uniform bondline. Conformable pads such as silicone rubber may be used to help distribute pressure. Screw clamps are not generally recommended. Weights are effective for small parts but become cumbersome for larger boards.

Vacuum Cure Option: Vacuum bag or Vacuum lamination press curing may be beneficial for some applications. Curing under vacuum can significantly reduce the risk of entrapping air in the bondline, thus helping to ensure the best thermal and/or electrical properties attainable. Less pressure may be required, as curing under a vacuum has been known to increase flow and substrate wet-out.

Controlling Flow: In the case of excessive resin flow or bleed, try one of the following alternatives:

  • Use a lower cure pressure
  • Have preforms made with edge cutback
  • Use a faster oven ramp rate

Poor Electrical Contact: In the case of poor electrical contact or grounding, an acoustic scan can verify if bonding is poor. If a poor interface is suspected, try these alteration to the cure profile:

  • Use a higher cure pressure
  • Use vacuum cure to prevent entrapped air
  • Ensure even distribution of pressure to eliminate any pinching or areas of low compression.

If after adjusting, grounding requirements are still not met, it may be necessary to try a more conductive product. Films without a fiberglass support, such as LOCTITE® ABLESTIK CF 3350 or LOCTITE® ABLESTIK 5025E, are generally more conductive.

Exposing to Solder Reflow: While exposing a cured application to solder reflow temperatures is not generally recommended, it is often necessary. In these situations, please follow the guidelines listed below for the best outcome. The following chart lists products that show minimal degradation at listed peak temperatures. Exposure time is expected to be around 30 seconds. Products may withstand higher temp exposures if the duration is kept short.

Temperature Range Products
Low (Below 200°C) 561, 561K, 566, 566K, 5662, 506, ECF561, ECF561E
Mid (Up to 230°C) 563K, ECF563, CF3350, 5025E, CF3352
High (Up to 270°C) ECF568, 550K, CF3366

Exposing film to solder reflow temperatures may result in weakening of the bond an/or reduction in electrical and thermal conductivity. Slower ramp rates may help reduce complications as will the use of smaller boards.

High Frequency Applications: Proper grounding for high frequency RF applications may require special film characteristics. For this type of application, LOCTITE® ABLESTIK CF 3350 or LOCTITE® ABLESTIK 5025E are highly recommended for their uniformity and high conductivities.

 

Common Applications for Assembly adhesive films

Aerospace
Mechanic standing behind wheel near engine and beneath wing of a parked airplane with desert background

High-reliability film adhesive solutions for aerospace electronics in planes, helicopters, and unmanned aerial vehicles (UAVs) including engines, turbines, sensors, guidance systems, and navigation systems.

Radar/Sonar
Photo of large grey satellite dish with blue sky and clouds in the background cropped shutterstock ID 22571947

Proven and trusted epoxy film adhesive solutions supporting high-reliability radar and sonar assemblies including antennas, phase shifters, T/R modules, power modules, transmitters, and sensors.

Satellite
Shutterstock photo of space satellite orbiting a blue earth with white clouds

High-reliability film adhesives supporting satellite assembly including directed energy, communication, guidance, navigation, and control systems.

Optically clear assembly films

KRAYDEN's ITO (Indium Tin Oxide) film and OCA (Optically Clear Adhesive) are designed for use in a variety of optically clear applications. ITO and OCA films are a critical part for modern electronic devices, providing transparent and conductive solutions.

Indium Tin Oxide films: ITO conductive film, constructed on a PET substrate, is formulated by depositing Indium Tin Oxide with the rare metal Indium as the primary raw material onto a PET film. Functioning as an n-type semiconductor material, ITO conductive film exhibits a remarkable combination of high self-carrier concentration (low resistivity), wide band gap, and superior light transmittance within the visible spectral region. This unique set of properties makes ITO conductive film indispensable in numerous applications, prominently in flat panel display devices and solar cells.

Optically Clear Adhesive films: Optically Clear Adhesive serves as a specialized bonding agent for transparent optical components like touchscreens and lenses. This adhesive is designed to meet specific criteria, including transparency, a light transmittance exceeding 90%, robust bonding strength, room-temperature or medium-temperature curing, and minimal curing shrinkage. OCA is a fundamental raw material for touch screens, particularly as a double-sided adhesive tape with matrix-free material. The matrix-free construction involves transforming acrylic glue into a matrix-free form and subsequently attaching a release film to the upper and lower layers. Notably, optically clear adhesive is categorized into resistive OCA and capacitive OCA, each tailored for specific applications.

 

Common Applications for Optically Clear Assembly Adhesive Films

Displays
ITO used for its exceptional conductivity and transparency
ITO conductive film's exceptional conductivity and transparency make it a cornerstone in the manufacturing of high-quality displays for devices like smartphones, tablets, and monitors.
Touchscreens
OCA ensure seamless bonding between transparent layers
OCA, as a critical component in touchscreens, ensures seamless bonding of transparent layers, enabling responsive and clear touch functionality.
Solar Cells
ITO solar cells contribute to efficient light transmittance and electrical conductivity
The utilization of ITO conductive film in solar cells contributes to efficient light transmittance and electrical conductivity, enhancing the overall performance of solar energy conversion.
 

Leading Brands Trust in Our Products and Services