Instant Adhesives

One-Component & Low-Viscosity

Instant Adhesives

Instant adhesives, commonly known as cyanoacrylates or super glues, cure in seconds through a moisture-triggered anionic polymerization rather than solvent evaporation or heat. A thin film of surface moisture, present on nearly all substrates, is enough to trigger the reaction, making these one-part, no-mix systems ideal for fast-turnaround assembly, prototyping, and repair work.

Ethyl cyanoacrylates are the general-purpose workhorse of the family, offering fast fixture times and strong adhesion across plastics, rubbers, metals, and most porous and non-porous substrates. Methyl cyanoacrylates cure even faster and typically deliver higher bond strength on metals and less porous materials, though they can be more brittle and prone to surface blooming (frosting) on some plastics. Both chemistries are available in a range of viscosities, from water-thin formulations that wick into tight-fitting joints to gel and thickened grades formulated for vertical surfaces and gap-filling applications.

100 products

RecommendedPrice low to highPrice high to low
  • LOCTITE 401

    LOCTITE 401

    • Instant adhesive
    • Very high adhesion strength
    • Bond dissimilar substrates
  • 3M™ Fastbond™ 2000NF

    3M™ Fastbond™ 2000NF

    • Quick bonding without heat
    • Immediate handling strength.
    • Post-formable and heat resistant
  • Loctite 495

    Loctite 495

    • One-Part Adhesive Form
    • Multi-Substrate Assembly Fixturing
    • Low-Viscosity Adhesive Application
  • PERMABOND 105

    PERMABOND 105

    • 5 to 20-Second Fixture Time
    • Low-Viscosity Single-Component Adhesive
    • Hard-to-Bond Plastic and Rubber Bonding
  • PERMABOND 2011

    PERMABOND 2011

    • Thixotropic Application Control
    • 5 to 10-Second Fixturing Time
    • One-Part Moisture-Cure Adhesive
  • 3M CA40H

    3M CA40H

    • Higher-Viscosity Controlled Dispensing
    • EPDM, Vinyl, and Aluminum Bonding
    • Alignment-Friendly Slower Set Time
  • CYBERBOND 2241

    CYBERBOND 2241

    • Toughened Structural Bonding
    • Metal, Plastic, and Rubber Bonding
    • Up to 140 deg C Service
  • LOCTITE 382

    LOCTITE 382

    • One-Component Adhesive System
    • Clear Gel Formulation
    • Gap-Filling Cyanoacrylate Bonding
  • LOCTITE 4013

    LOCTITE 4013

    • Medium-Viscosity Cyanoacrylate Adhesive
    • ISO 10993 Biocompatibility
    • Disposable Medical-Device Assembly
  • LOCTITE 403

    LOCTITE 403

    • Low-Odor Bonding Processing
    • Low-Blooming Bonding Cure
    • High-Viscosity Placement Control
  • LOCTITE 404

    LOCTITE 404

    • Optically Clear Bondline
    • Fast Adhesive Cure
    • Low-Viscosity Adhesive Application
  • LOCTITE 4081

    LOCTITE 4081

    • Very-Low-Viscosity Cyanoacrylate Adhesive
    • Low-Odor Adhesive Cure
    • Disposable Medical-Device Assembly

Frequently asked questions

Frequently Asked Questions about Instant Adhesives

What is the difference between cyanoacrylate and "super glue"?

There is no chemical difference. Cyanoacrylate is the technical name for the polymer chemistry, while super glue is the common consumer term for the same class of instant adhesives. Industrial-grade cyanoacrylates are formulated with tighter viscosity control, extended shelf life, and application-specific properties not typically found in consumer-grade products.

What is the difference between ethyl and methyl cyanoacrylate?

Ethyl cyanoacrylate is the most widely used general-purpose grade, offering a good balance of cure speed, flexibility, and broad substrate compatibility. Methyl cyanoacrylate cures faster and often bonds more aggressively to metals and rigid, low-porosity substrates, but it tends to be more brittle and is more prone to blooming, a visible white haze that can form around the bond line from vaporized, unreacted adhesive. The right choice depends on the substrate, required bond strength, and whether cosmetic appearance matters.

Why does cyanoacrylate cure so quickly without mixing or heat?

Cyanoacrylate monomers are highly reactive to weak bases, and the trace moisture naturally present on almost every surface is enough to initiate anionic polymerization. Once triggered, the monomer chains link together in a chain reaction that completes in seconds to minutes, depending on the substrate, bondline thickness, humidity, and ambient temperature.

Why do some porous substrates cure slower or fail to bond well?

Highly porous or very dry substrates can absorb the adhesive into the material before enough surface moisture is available to trigger a full cure, sometimes leaving uncured monomer starved of the moisture it needs to polymerize completely. This can result in a weaker bond or an incomplete cure at the interface. Thicker or gel-viscosity cyanoacrylates, or the use of a compatible primer, can help address this on porous or absorbent substrates.

What causes the white haze or "blooming" around a cyanoacrylate bond?

Blooming occurs when cyanoacrylate vapor from the curing adhesive condenses on nearby surfaces and polymerizes on contact with moisture in the air, leaving a visible white residue around the bond line. It is more common with fast-curing, low-viscosity grades and in enclosed or poorly ventilated spaces. Lower-bloom formulations, adequate ventilation, and controlled dispensing can reduce this effect.

When is an activator or primer needed with cyanoacrylate adhesives?

Activators and primers are used when the substrate lacks sufficient surface moisture or reactive chemistry to cure the adhesive on its own, such as with certain low surface energy plastics, or when a near-instant, full-depth cure is required regardless of ambient humidity. An activator is typically applied to one surface before the adhesive is applied to the other, accelerating and deepening the cure through the full bondline.

Are cyanoacrylate bonds flexible or impact-resistant?

Standard cyanoacrylates form rigid, glassy bonds that offer excellent tensile and shear strength but limited flexibility, making them prone to failure under sudden impact or repeated flexing. Rubber-toughened cyanoacrylate formulations are available for applications requiring greater peel strength and impact resistance, trading some rigidity and heat resistance for improved durability under dynamic loads.

How well do cyanoacrylate bonds hold up to heat?

Standard cyanoacrylates typically have a lower continuous service temperature range than epoxies or structural acrylics, and prolonged exposure to elevated temperatures can degrade bond strength over time. Specialty high-temperature-resistant cyanoacrylate grades are available for applications that need to withstand higher sustained heat, though they generally still fall short of epoxy or silicone performance at extreme temperatures.


Learn more

Instant Adhesives: Ethyl & Methyl Cyanoacrylates

Instant adhesives cure in seconds through a moisture-triggered reaction rather than solvent evaporation or heat. A thin film of surface moisture, present on nearly all substrates, is enough to trigger polymerization, making these one-part, no-mix systems ideal for fast-turnaround assembly, prototyping, and repair work.

Ethyl cyanoacrylates are the general-purpose workhorse of the family, while methyl cyanoacrylates cure even faster and typically bond more aggressively to metals and low-porosity substrates, at the cost of some flexibility and a higher tendency to bloom.

Instant adhesive bonding

Ethyl vs Methyl Cyanoacrylate Selector Guide

Both chemistries cure by the same mechanism; the choice comes down to substrate, cure speed, and cosmetic requirements

Ethyl Cyanoacrylate
Cure Speed
★★★★☆
Flexibility
★★★★☆
Blooming Risk
★★★☆☆
Metal Adhesion
★★★☆☆
Substrate Range
★★★★★
Best for general-purpose bonding, plastics, rubbers, mixed substrates
Methyl Cyanoacrylate
Cure Speed
★★★★★
Flexibility
★★☆☆☆
Blooming Risk
★★☆☆☆
Metal Adhesion
★★★★★
Substrate Range
★★★☆☆
Best for metals, rigid low-porosity substrates, fastest fixture time

Key Performance Considerations

Moisture-Triggered Cure

No mixing or heat required. Trace surface moisture is enough to trigger cure in seconds to minutes, depending on bondline thickness and ambient humidity.

Porous Substrate Limits

Highly porous or very dry substrates can absorb adhesive before enough moisture triggers a full cure, sometimes weakening the bond. Gel grades or primers can help.

Rigid, Low-Flex Bonds

Standard grades form rigid, glassy bonds with strong tensile and shear strength but limited flexibility. Toughened, rubber-modified grades trade some rigidity for impact resistance.

Bloom & Blush

Vapor from curing adhesive can condense and haze nearby surfaces, especially with fast, low-viscosity grades in enclosed spaces. Low-bloom formulations reduce this.

Core Applications

Electronics Assembly

Tacking small components, wire staking, and rapid fixture during PCB assembly where clamp time isn't available.

Plastics & Rubber

Fast-turnaround bonding of housings, gaskets, and molded parts in prototyping and production repair.

Metal Fabrication

Rapid tacking of small metal parts before welding, or as a standalone bond for low-load metal assemblies.

MRO & Field Repair

Quick fixes on the shop floor or in the field where clamping equipment or long cure windows aren't practical.

Need Help Selecting the Right Instant Adhesive?

Chemistry selection depends on your substrate, required fixture time, flexibility needs, and whether bloom or cosmetic appearance matters. Our technical team provides product selection support, trial quantity sourcing, and application guidance across ethyl and methyl cyanoacrylate systems.

Instant Adhesive – Quick Reference

Ethyl CAGeneral purpose, flexible, broad substrates
Methyl CAFastest cure, strongest on metal, more brittle

Leading Brands Trust in Our Products and Services