Liquid Encapsulants

Encapsulants for electrical insulation and mechanical protection

Liquid Encapsulants

Liquid encapsulants are much more flexible than traditional Epoxy mold compounds, removing the need for expensive molding machines and molding plates. This way, they allow manufacturers to produce smaller and and more flexible batches, making the products better suited for diverse low quantity orders. Optical grade encapsulants can also have efficient application in LED encapsulation.

Encapsulants are primarily used to ensure environmental protection and boost the mechanical strength of wire bonded devices. They are developed to provide protection to wire bonds, leads and aluminum.

Encapsulants deliver unmatched performance for a variety of products including transistors, system in package (SIP) devices, ASICs, and chip-on-board applications. Cycle time and costs can be reduced through the use of glob tops. These materials for chip-on- board applications are designed to cure quickly to fit easily within high-speed manufacturing operations.

Liquid encapsulants are formulated and tested in-process and in the context of full package assembly. They meet the most stringent JEDEC-level testing requirements and are developed to deliver outstanding performance within high temperature lead-free environments. Krayden offers a wide range of Liquid Encapsulants. We are proud to offer Henkel\'s entire LOCTITE product line but also our own LinqSil and Optolinq products.

180 products

RecommendedPrice low to highPrice high to low

Product selector guide

The table below gives a quick overview of our current leading products for liquid encapsulation. Please scroll below for the entire encapsulation range.

Leading Encapsulant Adhesives
  FIL7010C FP 4470 FP 4450HF FP4802 FP 4651 FP 4653 FP 4451TD DAM 7010C
Color Black Black Black Black Black Black Black Black
Viscosity 25,000 42,000 32,000 80,000 >100,000 >100,000 300,000 92,500
Silica Filler % 80 75 73 72 82 86 73 80
Max filler size, um 120 50 25 50 50 75 200 120
SVHC FREE YES YES FREE YES YES YES FREE
Ionics level, ppm <10 <2 <2 <5 <5 <10 <10 <10
Tg by TMA, °C 135 - 145 148 164 50 150 150 150 135 - 145
CTE1 16 18 21 20 11 7 21 16
CTE2 58 65 72 100 50 NA 65 63
Cure time, min(2 steps) 60 + 60 30 + 90 30 + 90 30 + 90 60 + 90 150 + 150 30 + 90 60 + 60
Cure temperature °C 100 + 150 125 + 165 125 + 165 125 + 165 125 + 165 110 + 150 125 + 165 100 + 150
Pot life at 25°C 1 3 4 0.33 2 1 10 1
Shelf life at -40°c, months 6 9 9 9 9 9 9 6
Encapsulant Type      FILL DAM

 

Encapsulant Adhesives
Product Apps and Attributes Viscosity at 25°C (mPa.s) Filler Type (Content) Max Filler Size, um Hardener type Tg by TMA (°C) CTE α1(ppm/°C) CTE α2(ppm/°C) Cure time (min) Cure Temp °C
Dam
LINQBOND LB-DM801 Designed to work in conjunction with LB-FL501 as a dam material for semiconductor packaging. 42,000 - - - 139 20 60 40+20 150 + 160
Loctite ECCOBOND 7010C DAM Protection of bare IC, Well defined height 92,500 Silica (80%) 120 SVHC free 140  16 63 60 - 60 100 + 150
Loctite ECCOBOND EO 7029 Smartcard encapsulation and die attach 48,000 - - - 110  66 181 5 150
Loctite ECCOBOND FP4451TD BGA and memory encapsulation. Highest aspect ratio for Tall Dam 300,000 Silica (73%) 200 Anhydride 150 21 65 30 + 90 125+165
Loctite ECCOBOND FP4451 Discontinued - No longer available 300,000 Silica (72%) - Anhydride 155 22 - 30 + 90 125+165
Fill

LINQBOND 
LB-FL501

One-component fill epoxy encapsulant specifically designed for rapid temperature fluctuations 37,000 - - - 180 23 77 30 + 90 135 + 175
Loctite ECCOBOND 7010C FIL Potting or encapsulation protection for stress sensitive components 25,000 Silica (80%) 120 SVHC free 140 16 58 60 + 60 100 + 150
Loctite ECCOBOND FP0087 Stress-sensitive devices and severe automotive environments 20,000 at 20 rpm Silica (76%) N/A Anhydride 175 18 69 60 + 60 125 + 180
Loctite ECCOBOND FP4450 Discontinued - No longer available 44,000 Silica (73%) 120 Anhydride 155 22 72 30 + 90 125+165
Loctite ECCOBOND FP4450HF Automotive, BGA, memory, COB, SIP and SmartCard 32,000 at 20 rpm Silica (73%) 25 Anhydride 164 19 71 30 + 90 125+165
Loctite ECCOBOND FP4470 BGA, CSP, and full array on low temperature co-fired ceramic (LTCC) 48,000 Silica (75%) 50 Anhydride 148 18 65 30 + 90 125+165
Loctite ECCOBOND FP4650 High purity and low thermal expansion 325,000 Silica (83%) - - 140 15 - 60 + 120 120 + 160
Loctite ECCOBOND FP4651 Automotive, BGA, memory, COB, SIP, SmartCard and chip array ceramic packages 130,000 at 20 rpm Silica (82%) 50 Anhydride 150 12 50 60 + 90 125+165
Locite ECCOBOND FP4653 Chocolate breakable on pre-scored ceramic substrate 85,000 Silica (86%) - - 150 7 - 120 + 120 110 + 150
Loctite ECCOBOND FP4654 Discontinued - No longer available 32,000 at 20 rpm Silica (80%) 50 Anhydride 146 13 53 30 + 90 125+165
Loctite ECCOBOND FP4802 BGA, CSP and full array on low temperature co-fired ceramic (LTCC) 80,000 at 10 rpm Silica (72%) 50 Phenolic 50 20 100 30 + 90 125+165
Loctite STYCAST A316-48 Automotive grade potting material with High Tg for sensors and control modules 50,000 Oxide  - Amine 145 55 155 30 + 120 100
Glob Top
LINQBOND
GT2301
Provides excellent protection against moisture and vibration 65,000 - - - 130 50 160 40 120
Loctite ABLESTIK ME 995-1-4 Thermally conductive glob top 205,000 Silica - - 110 45 - 60 150
Loctite ECCOBOND EN 3838T Low temperature cure PCB protection 6,700 - - - 2 57 217 8 130
Loctite ECCOBOND EN 3915T Low CTE for flip chip device aplications 22,000 - - - 130 24 103 7 160
Loctite ECCOBOND EO 1016 Encapsulation of smart cards and watch ICs 62,000 Alumina N/A Amine 126 46 140 20 150
Loctite ECCOBOND FP4323 COB and plastic PGA encapsulation 220,000 at 2 rpm Silica (65%) - - 174 28 - 240 or 60 150 or 170
Loctite ECCOBOND FP4460 Automotive, BGA, memory, COB, SIP and SmartCard 300,000 at 10 rpm Silica (75%) 120 Anhydride 173 20 70 180 150
Loctite ABLESTIK 8387BM Discontinued - No longer available 14,000 PTFE, Silica 10 Hybrid Epoxy 122 88 168 5 or 60 150 or 100
Loctite ECCOBOND 50300HT Wire bonded bare die encapsulation 130,000 Silica (68%) 150 Anhydride 140 20 - 60 + 60 120 + 150
Loctite ECCOBOND 50300-1 Wire bonded bare die encapsulation 100 Silica(70%) - - 140 20 - 120 150
Loctite ECCOBOND 50300LT Wire bonded bare die encapsulation 55 Silica (69%) - - 140 20 - 120 150
Loctite ECCOBOND 50400-1 Wire bonded bare die on epoxy laminates 40,000 at 20 rpm Silica(70%) 150 Amine 140 20 - 60 + 60 120 + 150
Loctite ECCOBOND FP4660 CSP and low stress applications 120,000 at 5 rpm Silica (80%) 120 Anhydride 135 13 56 30 + 90 125+165
Loctite ECCOBOND UV8800M Discontinued - No longer available 2,500 - 4,000 at 5 rpm Silica (54%) 21 - 29 41 135 2 seconds 315 - 400 nm (UV)
Loctite ECCOBOND UV8800M-X Discontinued - No longer available 3,400 - - - 47 48 149 30 sec 100 mW/cm2
Loctite ECCOBOND UV 9052 UV cure for inkjet applications 41,000 - - - -  - - 5 - 10 sec 0.5 - 1 J
Loctite ECCOBOND UV 9060F Protection of WLCSP and BGA 11,000 - - - 75 81 198 5 - 25 sec  300 w/In
Loctite EO7021 CSP, BGA and SmartCard encapsulation 17,000 at 5 rpm - - - 125 67 187 60 or 5 120 or 150
Loctite SI 5088 UV and moisture cure for gasketing and sealing on glass, metals and ceramics 65,000 Unfilled - Silicone - 3 -  Mix Mix
Loctite SI 5293 UV cure silicone for PCB protection - - - Silicone -40 300 - - -
Loctite STYCAST 2851FT Solvent free encapsulant 85,000 - - - - 31 - 60 120
Loctite STYCAST SC3613 LED display coating and IC hybrid passivation 3,500 Unfilled - Silicone - - - 30 + 60 120 + 150
Loctite STYCAST U2500 For transformer PCBs and insulation apps 6,000 Polyurethane - - -53 155 - 240 60

Frequently asked questions

Frequently Asked Questions about Liquid Encapsulants

How do I choose the correct needle for dispensing filled materials, and what should I expect during curing?

For filled materials, select a nozzle ID ≥ 3× the maximum particle size of the encapsulant. Example, for FP4451TD (median ~20 µm, max ~200 µm): 20G (0.60 mm), 18G (0.84 mm), or 16G (1.19 mm). Always validate your chosen needle over a production run for dispensing consistency. 

Do you have UV cured silicones with high refractive index?

We don't have high refractive index materials that cure with UV. The UV activators required limit transmission, and UV exposure can damage the silicone, causing yellowing and further reducing transmission. UV-cured silicones are generally not suitable for high-transmission, high-refractive applications.

What causes bubbles in my encapsulant?

Most bubbles are not caused by the encapsulant itself. For solvent-based materials, outgassing can occur, but in 100% solid systems like FP4450 and FP4451TD, outgassing is negligible. Bubbles usually originate from moisture in the substrate. Prebaking the substrate or storing it in a dry box prevents bubble formation.

What is substrate prebaking?

Prebaking removes moisture from substrates previously exposed to humidity. Typical prebaking: 100°C for 1 hour. After prebaking, follow the recommended dispense and cure steps in the TDS. Alternatively, store substrates in a dry box or use a lower temperature step-cure if prebaking is not feasible.

How do I know when my product is fully cured?

Materials are fully cured after following the recommended cure schedules in the TDS. Differential Scanning Calorimetry (DSC) cure kinetics can be used to confirm complete curing.

How many volts can liquid encapsulants typically withstand?

Typical silica-filled encapsulants withstand 500–1000 V/mil (20–40 kV/mm). For higher voltages, verify the electrode gap, not just encapsulant thickness, to ensure proper insulation.

 What are PCB/Component protection encapsulants?

PCB protection encapsulants shield passive components (capacitors, resistors) from dust, moisture, and mechanical impact. Examples include LOCTITE ECCOBOND 3838T (black low-modulus epoxy), UV9060F (light blue UV acrylate with moisture cure), ABP 6892 (clear epoxy), clear silicones 8035 and STYCAST SC 3613, and LOCTITE 3217 (UV/heat dual-cure).

For better encapsulant retention, a DAM may be needed. Recommended options include black ABP 8420 epoxy, black ABP 8142B silicone, or thixotropic LOCTITE 3621 red epoxy and LOCTITE 3217, which can be UV cured before the fill operation.


Learn more

Liquid Encapsulants

Epoxy Mold Compound vs Liquid Encapsulation

There are two main ways to encapsulate a semiconductor device: transfer molding a thermosetting Epoxy Mold Compound (EMC) or using liquid encapsulation directly on the Printed Circuit Board (PCB). Encapsulation in EMC is better than liquid encapsulation for applications that require higher filler content, and for the same reason, volume for volume, EMC is usually cheaper than liquid.

Liquid encapsulation, on the other hand, has a high flexibility and low throughput

Liquid casting is however much more flexible. EMC requires are large significant investment in molding machines and mold plates for specific devices which must produce large quantities before there is a return on that investment. Liquid encapsulation on the other hand has a high flexibility and low through put: meaning that it is best suited for a multiple diverse low quantity orders.

glob top and dam n fill encapsulation
Liquid resins are used in two main ways in encapsulations processes: glob top and dam & fill alternatively known as frame & fill
glob top image
Liquid resin encapsulation via the glob top process is a single step application process but is less precise than dam & fill

In general liquid encapsulation is used for LEDs and potting or encapsulating electronics in bare die mounting on printed circuit boards (PCB), otherwise known as chip on board (COB).

Another advantage of potting and encapsulating devices in liquids is that in general, the result is flatter and thinner than devices encapsulated by a transfer molding process around a lead-frame with EMC. The space requirements for devices will continue getting more and more stringent as the component density of devices increases. This trend makes encapsulation and potting in liquids a sure bet for the future.

Transfer molding EMC may also cause wire sweep: where the pressure of the flowing molten compound shifts the fine-pitched bonding wires connecting a die. Wire sweep can cause shorts and mutual inductance. Liquid encapsulation is applied from above and does not disturb bonding wires. That’s why it is the industry standard for larger or extra sensitive dies and chips.


Liquid Epoxy: Viscosity and Thixotropy

Bare die may be mounted to the PCB with die attach but that’s not enough to protect them or their connecting wires from moisture, mechanical stress, temperature, and chemical corrosion. That’s why it makes sense to insulate and encapsulate them with a protective potting layer of liquid encapsulant.

The low viscosity of liquid encapsulants is good for flat smooth finishes.

In non-Newtonian thixotropic encapsulants thixotropy refers to the temporarily lower viscosity of an epoxy gel when shear, pressure, or temperature is applied. This means that they can be gel-like when at rest, but flow like a liquid when agitated.

Being able to control the viscosity of liquid encapsulants means you can dial in how far they will spread over a surface area, and also how high they will build up to. This is important in Glob Top encapsulation where devices are literally encapsulated by a “Glob” from above.

dam and fill processDam & Fill or Frame & Fill is a two step encapsulation process that is a little like 3D printing

Glob Top vs Dam & Fill

GlobTopVSDamFill

Glob Top is a process of encapsulation by using a fluid encapsulant gel with higher viscosity so that it fully encapsulates a device without flowing beyond the necessary area. As mentioned, by controlling the temperature, shear, and pressure, the viscosity and flow of liquid can be adjusted so that the final surface area and height of the “Glob” can be controlled quite effectively.

Dam & Fill on the other hand refers to a two-step process of encapsulation, where a ring or frame of higher viscosity liquid encapsulant is applied as a “Dam” around a device, and then a lower viscosity liquid “fill” is used to then fully encapsulate a device. The liquid used to build the frame or dam usually has more abrasive filler and a higher viscosity at rest than the liquid used for the fill.

Dam & Fill is a more selective protective coating and can be framed to cover areas in specific shapes, and is for example also used for optical bonding. In optical bonding the frame or dam is used to create a space between the glass and the display or touch screen. Then an optically clear fill is used as an adhesive and fixative.

Liquid Encapsulation for LEDs and Optoelectronic Devices

Optically clear liquid encapsulation is also used for LED devices, and encapsulate optical or optoelectronic devices that require both a high level of light transmittance as well as a good level of mechanical protection. In a similar process to Glob Top encapsulation, a literal glob of clear encapsulant is dropped directly into place on top of the LED. In another production process, optically clear liquid encapsulant is used to cast LED’s final body. Phosphor, colored dyes, and diffusant concentrates can be added to the liquid encapsulant to alter its optical properties.

Presentations

2026 Encapsulants

This presentation introduces encapsulant materials used to protect electronic components and assemblies from moisture, contaminants, vibration, and mechanical stress. It covers encapsulant chemistries, key performance characteristics, application methods, and material selection considerations for enhancing the reliability and long-term durability of electronic devices across industrial, automotive, and consumer applications.

2026 Materials for Optoelectronic Applications

This presentation provides an overview of advanced materials used in optoelectronic applications, including adhesives, encapsulants, thermal interface materials, and optical bonding solutions. It explores material requirements for LEDs, displays, optical sensors, and photonic devices, with a focus on optical clarity, thermal management, environmental protection, and long-term performance in demanding operating environments.

Related Blogs

Guardian Angel Blog

Encapsulants – Guardians of Integrated Circuits

This blog provides a comprehensive introduction to encapsulants, their applications, and why they are considered the guardian angels of integrated circuit assemblies.

Related Blog

Yellowing in Epoxy-Based Liquid Encapsulants

This blog talks about the mechanism behind the yellowing in epoxy-based liquid encapsulants and the strategies that can be adapted so as to prevent or minimize it. 

Related Blog 2

Better Thermal Conductivity in Encapsulants

A summary of the recent research effort carried out where the interdependence of thermal conductivity with crucial properties of polymer-based encapsulants was investigated

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers