Optoelectronic Mold Compounds

White and Clear compounds suitable for Optoelectronics and LEDs

Optoelectronic Epoxy Mold Compounds

Optoelectronic Mold compounds can replace a lot of existing technology in Ambient light sensors, lens filters and proximity sensors. They have a lower cost compared to traditional glass, since standard optical filters can often run into the hundreds of dollars. This is mainly because they require fewer process steps since no adhesive is needed, as the filter is incorporated into the encapsulant. Additionaly, they can have custom cut-off and bandpass with formulations tailored to your wavelength requirements.

White, highly reflective epoxy molding compounds, also abreviated as WMC, are epoxy molding compounds that are filled with a highly reflective filler that stays reflective even after exposure to  heat and UV for long periods of time. We offer a range of highly reflective, white, non-yellowing epoxy mold compounds for led packages and lighting applications that require a high-performance non-yellowing compound with high brightness and reflectivity.

Clear epoxy Mold compounds have different filler and chemistry than most common EMCs. Optically clear compounds are also used for LED devices, and to encapsulate optical or optoelectronic devices that require both a high level of light transmittance as well as a good level of mechanical protection. In a similar process to Glob Top encapsulation, a literal glob of clear encapsulant is dropped directly into place on top of the LED. In other production processes, optically clear compounds are used to cast the LED’s final body. Phosphor, colored dyes, and diffusant concentrates can be added to this liquid encapsulant to fine tune it to your needs and alter its optical properties.

21 products

RecommendedPrice low to highPrice high to low

Product selector guide

Optoelectronic Epoxy Molding Compounds
Product Name Key Properties
Color Specific
Gravity
Glass Transition
Temperature (Tg), °C
CTE, Alpha 1
ppm/°C
CTE, Alpha 2
ppm/°C
Moisture absorption Gel time (s) Refractive index Spiral flow (cm)
BMC-1100 Black 2.1 150 20 50 - - - 70-160
BMC-4200 Black 1.22 115 8 21 - 20-50 - 80-240
Hysol GR17 White 1.75 182 26 66 0.46% 25 - 50
Hysol GR180R White 2.02 203 15 46 0.45% 19 - 68
Hysol GR180T Clear 1.85 195 26 67 0.67% 15 - 73
Hysol GR300S Black 1.9 169 15 52 0.35% - - 84
TC 7600H BDF Black 1.56 135 50 120 - 25-45 1.56 150-250
TC 8020LS White 1.2 95 70 220 0.17 20-40 - 150-250
TC 8020T Clear 1.23 - 70 170 0.45% 20-40 1.56 150-250
TC 8040 Clear 1.22 135 81 175 - 20-45 - 150-250
TC 8060 Clear 1.3 160 85 180 - 20-40 1.56 150-250
TC 8090 Clear 1.28 140 74 200 - 20-40 1.53 150-250
TMC-2100 Clear 1.25 120 10 21 - - - 80-180
TMC-2100H Clear 1.20 110 6 17 - 35-60 - 80-180
TMC-2100IR Clear 1.20 110 4 17 - 25-50 - -
TMC-3282 Clear 1.24 125 70 185 - 35-60 - -
TMC-3282SF Clear 1.24 165 62 183 - 47.5 - 100-240
TMC-G373H Clear 1.15 100 60 80 0.25 25-50 1.56 80-220
WMC-1100 White 2.1 150 20 50 - 25-40 - 70-160

 

Legacy Optoelectronic Epoxy Molding Compounds - No longer available from KRAYDEN
Product Name Key Properties
Color Specific
Gravity
Glass Transition
Temperature (Tg), °C
CTE, Alpha 1
ppm/°C
CTE, Alpha 2
ppm/°C
Moisture absorption Adhesion to Ag/Cu/ NiPdAu Refractive index Tensile Strength (MPa)
OG10-1 Clear - 140 77 162 - - 1.53 110
OP1000 Clear - 139 80 161 0.48%  25/5/50 1.53 110
OC10-1 Clear - 142 75 163 0.44% 41/20/39 1.53 121
OL10-1 Clear - 147 70 167 0.25% - 1.52 136
OP7000 Clear 1.28 140 79 160 0.45% 20/20/37 1.52 110
OP70-2 Black 1.28 137 81 161 0.49% 46/27/56 - 94.5
2933-102A Clear - 151 41 90 0.2% - - 107
2912-58C White - 132 42 110 0.22% - - 100
OL88-8 Clear 1.28 139 80 161 0.25% - 1.51 -

 

Pelletizing capabilities
Diameter (mm) Weight  Height  Packing
13 0.15 1.90 - 3.90  0.20 12 - 25 1.5 7-10 kg/box (1kg bags)
16  0.15 2.80 - 5.80 0.40 12 - 25 1.5 7-10 kg/box (1kg bags)
35 0.40 13.5 - 45 1.5 12 - 41 2.5 8-10 kg/box (1kg bags)
Powder  - - - - - 5 kg/box (0.5kg bags)

Please note that all bags are made from Aluminum foil and vacuum sealed to prevent moisture absorption

Frequently asked questions

How do the WMC get and stay white?

White epoxy molding compounds are filled with Titanium Dioxide (TiO2), a very white filler that gives the epoxy its very high brightness and reflectivity. Different grades of TiO2 give different degrees of reflectivity. 

The choice and grades of resin and hardener base, on the other hand, are responsible for maintaining the WMCs whiteness and hence reflectivity after exposure to heat or UV radiance.

What is the difference between reflectivity and transmittance?

Typically, in LED and other lighting applications, we are looking for high light transmission that endures after heat and UV exposure. Transmission is the amount of light that is allowed to pass through the material.

However, to increase light efficiency and output, we are looking for materials that  have a high reflectivity to get as much light as possible out of the device. Reflectivity is the amount of light rebounded off a surface that is neither absorbed nor transmitted.


Learn more

Epoxies vs Silicone for Clear Encapsulation

Molding compounds can act as silicone replacement since they exhibit superior mechanical properties and prevent common silicone issues from occurring. They have rigid, non tacky surfaces that minimize dust collection and do not limit the light output. Their increased adhesion to PPA/PCT guarantees consistent reflectivity and transmissivity. 

Silicones on the other hand are more prone to pressure issues where the movement of soft silicone can potentially break the delicate wire bonds or collect dust that reduces the light output for optoelectronic applications. Additionally, silicones are known to delaminate at the PPA/PCT interface and create dark spots that reduce the reflectivity and light output. To add insult to injury, suphur compounds are allowed to evaporate through silicone and potentially corrode the silver pad and as a result destroy the electrical contact.

Clear compounds with custom wavelength attributes
Clear compounds with custom wavelength attributes
Refractive index

Epoxies are also great alternatives to silicones in regards to their refractive properties. They are cost effective solutions for mid power LED encapsulation that retain a >90% transmittance rate @400-1600nm while also staying clear (non yellow) after thousands of hours at 105°C. Their refractive index is pretty much similar to expensive phenyl silicones so they are more efficient and can accomodate a reduced cost per lumen as well as increased lumens per watt. An overall improvement.

Non yellowing

To stay on the non yellowing matter, the color of the bulb is very important for larger led lamps. It is important not to tell the "old" lamps from the new by their color. That\'s why our epoxies offer minimal transmission loss and minimal yellowing at demanding operating conditions.

R-Tran indicates the light the passes as a straight line
R-Tran indicates the light the passes as a straight line

Sensor replacement
Old school glass optical sensors are expensive to manufacture and difficult to miniaturize. Their require an intricate process with multiple steps to create lens filters and sensors for light sensing electronics. Enter clear epoxies which can be used as a low cost glass replacement that is easy to handle and miniaturise while are also able to adjust to your wavelength requirements. Be it for automotive, biometric or consumer applications, our light filter technology allows for precise wavelength cut off values with excellent initial and long term transmittance.

And on the matter of transmittance, we offer low stress epoxies that preserve straight light transmission something extremely uncommon for low stress and high clarity epoxies that are usually compromised by their low stress additives. These low stress clear compounds have very low CTE as well as very low moisture absorption while also maintaining high optical transmittance in the range of 400 - 1600nm.

These compounds retain their R-Tran and consistently exhibit high UV transmittance even after multiple reflow passes. They are uniquely suited for SMT devices that typically require excellent transmission in the ultraviolet range.

Common applications of Ultraviolet light
Common applications of Ultraviolet light

Transmission, absorption and reflection

Clear epoxies require the highest possible initial transmission and need to maintain this high transmission after aging. Mainly used in low power and high wavelength applications, clear molding compounds are widely popular in fields where early transmittance onset, high transmittance and no discolouration are strict requirements.

That\'s why we offer products with the earliest transmittance onset in the UV region (280 nm), the highest transmittance in visible & IR wavelengths that are also non-yellowing after continuous elevated temperature exposure. Products that are used to protects displays against degradation from humidity, dust, and UV exposure and are field-tested for use in outdoor displays

Optically clear epoxies are tailored for use on sensors and opto couplers with a revolutionary customized chemical filter technology that achieves the desired cut-off and bandpass transmission. So , if it wasn\'t "clear" enough yet, clear epoxies need, above all, to be transmissive.

Schematic of transmission, absorption and reflection
Schematic of transmission, absorption and reflection

Absorption has no place in the Optoelectronics category. Since it reduces light efficiency and generates heat it can only have a negative impact for any optoelectronic device, making it a value that needs to be reduced as much as possible. Imagine a (non opto graded) Black epoxy. It wont reflect or transmit any light through it. That\'s absorption for you. 

Reflectivity on the other hand is highly sought after for housing LED applications. 95% of the time this concerns White epoxy mold compounds that are surrounding the clear compounds. White compounds need to be highly reflective both initially and after ageing and assist into making ideal opto packages. 

Particle Size Distribution

Key optical properties—such as high transparency, minimal haze, and stable refractive index—are achieved through careful control of resin chemistry and filler particle size.

A critical factor in the performance of clear molding compounds is their particle size distribution. Uniform, fine fillers help reduce light scattering and surface roughness, ensuring excellent optical clarity and a smooth mold surface. This also improves flowability and reduces internal stress during molding, preventing defects such as voids, warpage, or delamination. In optoelectronic packaging, where performance and reliability are tightly linked to material behavior, a controlled PSD ensures both moldability and long-term stability. As a result, clear molding compounds with well-engineered formulations offer the ideal balance of transparency, mechanical integrity, and processability for high-performance optical devices.

KRAYDEN Clear Molding Compounds exhibit the following typical particle size distribution.

 

The Particle Size Distribution (PSD) curve, plotted as cumulative percent passing versus particle diameter on a logarithmic scale, represents the typical profile of KRAYDEN’s powder for clear molding compounds. The material exhibits a well-graded distribution with a median particle size (D50) of 38.34 µm, indicating a balanced composition of coarse and fine particles. Key cut-off points, including D90 at 80.08 µm and D10 at 11.26 µm, reflect excellent flowability with minimal fines. The narrow distribution tails, with D97 at 104.2 µm and D03 at 5.3 µm, demonstrate tight control over both oversize and ultrafine particles. A significant portion of the material, 87.3 percent, falls below 75 µm, while 96.4 percent is under 100 µm, providing strong packing density and consistent moldability. With only 8.35 percent of particles below 10 µm and virtually none under 1 µm, the powder also offers reduced dusting and safer handling. This optimized PSD supports reliable performance in molding, coating, and filler applications by ensuring uniform dispersion and a smooth surface finish.

Combining White and Clear compounds into a package

White colored epoxy mold compounds with low CTE are designed for applications requiring high brightness and reflectivity, and are ideally combined with clear optoelectronic molding compounds with similar CTE resulting in amazingly CTE matched LED packages.

Matched CTEs minimize warpage and the associated failures. 

As you can see in the following images it is very important for substrates and materials to be CTE matched. This means that the Coefficient of thermal expansion needs to be similar if not identical. This way when the adhesive/encapsulant/you name it shrinks, the substrate will shrink for the same %. And the same goes for expansion. So in practice you will have two (or more) materials that shrink and expand together and do not cause fractures or structural issues within their bond/package.

clear compound shrinakge

A higher CTE material will shrink more during cooling, or expand more during heating.

  • This behavior causes warpage in the molded package.
  • If adhesion between two materials of mismatched CTE is poor, delamination may occur.
  • Even when adhesion is excellent, excessive thermal stress between materials with two different CTEs can lead to cracking or wire breakage.

Presentations

Clear Molding Compounds for Optoelectronic Applications

This presentation provides an overview of clear molding compounds developed for optoelectronic applications such as LEDs, optical sensors, and photonic devices. It discusses material properties including optical transparency, thermal stability, UV resistance, and environmental durability, while outlining key considerations for selecting molding compounds that maximize device performance and long-term reliability.

Troubleshooting Guideline for Clear Molding Compounds

This presentation serves as a troubleshooting guide for clear molding compounds used in optoelectronic packaging. It reviews common molding defects, their underlying causes, and practical corrective actions to improve process consistency, optical quality, and manufacturing yield while ensuring reliable protection of sensitive optoelectronic components.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers