Bismaleimides

Amorphous & Liquid Imide extended oligomers

Bismaleimides (BMI)

Bismaleimides or BMI resins are a class of thermosets that offer significant advantages over other thermoset materials such as epoxies, urethanes, polyester and phenolics. Bismaleimides can be used as additives or base resins in adhesives that are designed for high temperature resistance or even FCCL layered applications. When used as a base resin they can produce adhesives that are tough, flexible and demonstrate good peel strength.

Unlike other suppliers, KRAYDEN offers unique imide-extended BMI or X-BMI\'s which have polyimides, dianhydrides and diamines as their backbone. Even though they can be used on their own, Bismaleimides are more often blended with reactive co-monomers to produce unique material properties such as very low cure shrinkage, low stress, hydrophobic and very thermally stable thermosets.

Please continue to our Learn More section to learn more about what makes our BMI resins unique and how our imide-extended bismaleimides can allow you to formulate unique high-value formulations.

12 products

RecommendedPrice low to highPrice high to low

Product selector guide

Bismaleimides - Imide extended Oligomers
Product CAS Description Key attributes Appearance Viscosity Applications
BMI-689 682800-79-9 A unique very low viscosity BMI resin
  • Toughener
  • Hydrophobic
  • High adhesion *
  • Superior thermal stability
Yellow to Amber Liquid 1,500 ± 500 (25°C)
  • Base resin or additive in thermoset formulations designed for high temperature resistance
BMI-689M 1911605-95-2 A unique low viscosity liquid BMI resin
  • Low viscosity liquid BMI
  • Hydrophobic
  • Superior thermal stability
Dark Amber

5,000 ± 2000

  • use as an additive or base resin in adhesives that are designed for high temperature resistance
BMI-689C - A pre-catalyzed unique low viscosity liquid BMI resin
  • Pre-catalyzed
  • Low viscosity liquid BMI
  • Hydrophobic
  • Superior thermal stability
  • Solvent free
Yellow to brown Liquid

1,500 ± 500

  • use for thermal curing. A minimum of one hour at 150°C is a recommended starting point. Higher temperatures (up to 175 – 180°C) will result in significantly shorter cure time requirements.
BMI-1400 1224691-98-8 An amorphous, low molecular weight bismaleimide oligomer that exhibits good adhesion to a variety of substrates
  • Specialty formulated lower viscosity version of BMI-1700
Amber 6,500 ± 1,000 (60°C)
  • Film adhesives
  • Pre-applied adhesives
  • Adhesion to metal
BMI-1500 1290041-56-3 An amorphous, low molecular weight bismaleimide oligomer that exhibits good adhesion to a variety of substrates
  • Soluble in many reactive diluents
  • Hydrophobic
  • Superior thermal stability
  • High adhesion to various substrates
Amber Viscous liquid 20,000 ± 10,000 (60°C)
  • Film adhesives
  • Pre-applied adhesives
  • Adhesion to metal
BMI-1700 1224691-98-8 An amorphous, low molecular weight bismaleimide oligomer that exhibits good adhesion to a variety of substrates
  • Soluble in many reactive diluents
  • Hydrophobic
  • Superior thermal stability
  • High adhesion
Amber High Viscous Liquid 30,000 ± 10,000 (60°C)
  • Film adhesives
  • Pre-applied adhesives
  • Adhesion to metal
BMI-5000 Powder 921213-77-6 Imide-extended bismaleimide oligomer that exhibits excellent toughness in the cured state with intermediate cross-link density.
  • Low cross-link density
  • Non-tacky
  • Film-forming
  • Maleimide functional oligomer
  • Cures to a tough thermoset
  • Additive to enhance toughness in thermoset compositions
Light Yellow Powder N/A
  • Film adhesives
  • Thermally resistant adhesives
BMI-6000 - A curable, low DK and Df alternative to replace both the Kapton and adhesive layers in the manufacture of FCCL materials. It can be processed in a resin system as a solid or dissolved in a solvent.
  • Toughener
  • Hydrophobic
  • Super thermal stability
  • Good dielectric properties
  • Excellent workability
  • High Tg
  • Low CTE
Light Yellow Powder N/A
  • Adhesive layer when laminating FCCL applications
  • Adhesion promoter

Frequently asked questions

Are there new products under development?

We are developing a couple of R&D resins with some unique properties:

  1. FM46-100 is provided in a solvent solution (anisole) - after drying and "curing" it is a thermoplastic-appearing material with great elongation and the unique feature of returning to its original shape
  2. The second (unclassified) material has the unique feature that after being formed into a film and deformed (folded, rolled up, etc.), it will hold that shape until warmed where it will then return to its original shape.

Can I use BMI with Acrylates?

Absolutely. Acrylates and methacrylates are regularly used in combination with Bismaleimides to modify die attach properties.

Acrylates are preferred because of their rapid curing, high Glass transition temperature, good adhesion,variable viscosities and variable functional group contents (1,2,3... acrylate groups per molecule). Of course nothing comes without drawbacks that can appear as potential brittleness and reduced moisture and temperature resistance.

What mix ratio do I use when mixing BMI with epoxy resin or acrylic?

The good news and the bad news is that there is no easy answer. In our experience we have encountered very few compatibility issues so virtually all BMI/acrylate or BMI/epoxy ratios are available to the formulators - it\'s just a matter of what they want for the final properties of the adhesive. Successful formulations have been created using 9:1 ratios of BMI as well as 1:6 ratios.

The BMI strong points (low modulus, good temperature resistance, hydrophobicity and good dielectric properties) lend themselves to the adhesive when blended with epoxies or acrylates since they share a cure chemistry.  Therefore you can make adhesives with less stress, better moisture and temperature resistance but not totally lose the good aspects of an epoxy or acrylic chemistry.

How do I cure BMI systems?

BMI resins cure free radically - whether thermally by the use of an organic peroxide catalyst or even by UV if using a free radical generating photoinitiator. DMI's preferred thermal catalyst is dicumyl peroxide (CAS # 80-43-3). We recommend using ~2% by weight of the resin content of the formulation and then curing at ~175ºC for an hour.

Of course, these values are just starting recommendations and your application and formulation may require other settings. There are a number organic peroxides that work well to thermally cure the BMI and BMI/acrylate resins.

test?

BMI resins cure free radically - whether thermally by the use of an organic peroxide catalyst or even by UV if using a free radical generating photoinitiator. DMI's preferred thermal catalyst is dicumyl peroxide (CAS # 80-43-3). We recommend using ~2% by weight of the resin content of the formulation and then curing at ~175ºC for an hour.

Of course, these values are just starting recommendations and your application and formulation may require other settings. There are a number organic peroxides that work well to thermally cure the BMI and BMI/acrylate resins.

 


Learn more

Comparison between BMI based die attach and Epoxy based die attach

 

BMI

Epoxy

BMI/Epoxy

Modulus

●○○○○

●●●○○

●●○○○

Moisture absorption

●○○○○

●●●○○

●●○○○

Thermal stability

●●●●○

●●○○○

●●●○○

JEDEC level 1 / 260 °C

Yes

No

Yes

Adhesion to substrate

●●●○○

●●●●●

●●●●○

100% solids

Yes

No

Yes

Snapcure option

Yes

No

No

Material cost

●●●○○

●○○○○

●●○○○

 

Amorphous and liquid imide extended oligomers

BMI Curing Methods

DMI aliphatic BMI resins (689, 3000, 1500, 1400, 1700, 2500) can be cured in a number of ways:

1. Thermal Cure. The most preferred method that gives the most complete cure uses thermal free radical generating catalysts. These catalysts are mainly peroxides that decompose at given temperatures to initiate the polymerization. There are a number of available catalysts but our all-time favorite is Dicumyl Peroxide (DCP). When using about 2 wt% of the resin this material will cause the BMIs to start curing at about 140ºC, peak at about 155ºC. We suggest curing at 175ºC for an hour to insure a thorough cure. You can cure hotter/faster or slower/longer - it is important to experiment to determine the best setting for their application. Another favorite peroxide catalyst is Perkadox 16. This is a low temperature catalyst that starts to cure the resin below 100ºC. This is good for rapid curing adhesives (like die attach paste). The down side is the catalyzed material must be frozen, shipped in dry ice and the pot life will be much shorter than that of a DCP catalyzed system.

aliphatic resins
imide extended oligomers

2. UV Cure. The BMI products cure via free radical initiated polymerization. One may use a photoinititator (UV catalyst) to prompt curing of these materials. Our favorite is Irgacure IR 819. This catalyst provides the free radical groups necessary to polymerize the resins upon exposure to 500 - 1,000 mJ/cm2 i-line (365 nm) UV radiation. This is beneficial as it occurs at room temperature and keeps the stress levels low. (Many) Other UV catalysts can also be used.

3. Homocure. You can cure the BMI-689 and BMI-1400 simply by heating them above 220ºC for an hour or two and they will self cure (homocure). This is the least preferred method of curing because 1) it\'s really, really hot and few applications can tolerate the heat and 2) it provides a less thorough cure than other methods.

 

 

BMI recommended storage conditions and shelf life

We recommend storage of our liquid BMI resins at 5ºC or colder and away from sunlight (UV sources). For the solid resins we suggest room temperature storage and away from light. DMI warrants the performance of the materials (shelf life) for 1 year from the date of shipment of the products (not the date of manufacture) if stored per recommendations. This insures a guaranteed full year of use of the materials after receipt.

bismaleimide application

Presentations

Bismaleimides

This presentation introduces bismaleimide (BMI) resin systems, including amorphous and liquid imide-extended oligomers developed for high-temperature and high-performance applications. It explores the unique thermal, mechanical, and chemical properties of BMI materials, along with their use in advanced composites, aerospace, electronics, and other demanding environments where exceptional durability and heat resistance are required.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers