Reactive Silicones

Mono terminal and Bi terminal reactive silicones

Reactive Silicones

Reactive Silicones grant permanent silicone properties to organic materials and other polymers. They harness the excellent heat resistance, flexibility, and mold release properties of Silicones and impart them to Organic materials while also maintaining abrasion resistance, water repellency, and good oxygen permeability.

They enhance the oxygen permeability of contact lenses, water repellency is added to functional paints, and artificial leathers are made to slide more by diminishing abrasion resistance. Reactive silicones have a very narrow molecular weight distribution, and very low volatiles such as cyclic siloxanes, enabling uniform reactivity 

Reactive Silicones (Polydimethylsiloxanes, PDMS), depending on their functional group, can react with a variety of organic compounds. Amino reactive groups react with Amide, Imide and Epoxies. Hydroxy reactive groups react with Urethanes and Esters. Finally Methacryloxy reactive groups are compatible with Acrylic resins.

13 products

RecommendedPrice low to highPrice high to low

Product selector guide

Mono Terminal

Product Structural formula Molecular weight Specific gravity Viscosity
FM-0411P

Hydroxy

1,000 0.96 10 - 25
FM-0421 5,000 0.97 60 - 80
FM-0425 10,000 0.97 140 - 180
FM-DA11 Diol

1,000 0.97 50 - 70
FM-DA21 5,000 0.97 80 - 160
FM-DA26 15,000 0.97 300 - 700
FM-0711 Methacryloxy

1,000 0.96 7 - 13
FM-0721 5,000 0.97 54 - 79
FM-0725 10,000 0.97 150 - 260
TM-0701T Methacryloxy

423 0.91 2.9 - 6.1
FM-0815J

Alkoxysilyl

3000 0.96 20-30

 

Bi Terminal

Product Structural formula Molecular weight Specific gravity Viscosity
FM-3311

Amino

1,000 0.95 11 - 15
FM-3321 5,000 0.97 90 - 150
FM-3325 10,000 0.97 200 - 400
FM-4411 Hydroxy

1,000 0.97 30 - 40
FM-4421 5,000 0.98 100 - 125
FM-4425 15,000 0.97 250 - 400
FM-7711 Methacryloxy

1,000 0.98 14 - 20
FM-7721 5,000 0.98 30 - 100

 

Frequently asked questions

What is the content of Volatile components?


We have data on volatile components and low molecular siloxane in JNC products. The content is not zero, but it is generally very low. You can expect the values to be similar between FM-04 and FM-DA series. For example, if Silaplane is used for filler disperson, the required Silaplane for filler dispersion is ±3-5%, making the overall volatiles insignificant.

Why do we need Reactive functional groups?


Silicones with reactive functional groups can react with surfaces and resins and remain in the system. Non reactive silicones (ie Silicone oil) are not grafted or blocked in place with their functional groups, leading to extensive bleed out. This is a result of plain mixing and zero copolymerization happening between the resin and the Silicone. Mixing doesn't bind anything into place so bleeding can occur very easily. Therefore, the use of silicone with reactive functional groups can reduce bleeding.

 

What solvent is compatible between the reaction of Polyethylene group methacrylate with Silaplane to ensure polymerization?

 

The reaction mentioned can be a potential in the paint industry to developed an anti abravie property paint coat. To ensure polymerization and no phase separation to occur the solvent that is recommended is butyl acetate or any that has its solvent polarity (SP) equivalent. Furthermore, for the synthesis method, we recommend that the initiator should be introduced after thoroughly mixing the monomers (Silaplane and PEG methacrylate) with the solvent.

 

What is the Shelf life and Opened bottle pot life of JNC materials?

Before opening, the product is basically guaranteed for 6 months after shipping which have exceptions depending on the grade. Once the product has been opened, JNC does not guarantee its quality.


Learn more

Mono and Bi Terminals

Reactive Polydimethylsiloxanes have two main grades. Mono and Bi terminals, meaning they have a reactive site in one or both ends of the chain. Monoterminal silicones are used for grafting polymers while bi terminal types are used for block polymers.

Mono terminal Polydimethylsiloxanes are grafted onto the resin, modifying the surface properties while biterminal Polydimethylsiloxanes are integrated into the block polymer, modifying the physical properties. Their narrow molecular weight distribution ensures uniform reactivity and low volatiles and impurities.

 

Why do we need the Reactive functional groups?

Not reactive silicones (ie Silicone oil) are not grafted or blocked in place with their functional groups, leading to extensive bleed out. This is a result of plain mixing and zero copolymerization happening between the resin and the Silicone. Mixing doesn't bind anything into place so bleeding can occur very easily.

Filler Dispersion

One of the main applications of the mono terminal Silaplane, which has a linear chain resin, is the ability to make the inorganic filler easier to blend into the silicone binder resin. In other words, it facilitates filler dispersion.

It improves the flowability of the highly filled filler dispersions and facilitates their handling. It is a perfect fit for applications that would benefit from the introduction of higher filler content, such as Thermal Interface Materials.

The product's narrow molecular weight distribution ensures uniform reactivity, low impurities and also low volatiles. With this variability, we can fine tune the silicone and compatibility buttons and have a product that perfectly fits the best of both worlds.

The silicone functional group of our Reactive PDMS (Polydimethylsiloxane) has a very high affinity to bind on the silicone binding resin. This improves the wettability between the resin and the filler. Additionally, the repulsive force that is created between the fillers, stabilizes the dispersion. This is a result of the silicone repulsion and the osmotic pressure effect.

The material turns from a highly viscous fluid that is in an aggregated state to a low viscosity one in a dispersion state that flows easier while also retaining higher filler content than it otherwise could. This results in higher flowability compared to other common silane dispersants.

In practical terms this means two things:

  1. Reactive silicones can lower the viscosity while keeping the same thermal conductivity and filler ratio
  2. Reactive silicones can increase thermal conductivity by allowing an increase in filler content.

Filler dispersion applications can benefit from the grafting properties of Mono terminal PDMS and the repulsive force that is created between the fillers. That's why we suggest them for this type of application. Hydroxy and Diol Hydroxy functional groups lend themselves better as a filler dispersant and have been used successfully on TIM applications.

Silaplane molecular weight distribution is very narrow (~1.03-1.4 Mw/Mn compared to the 1.8 or higher of general reactive silicones) and you have a choice between compatibility and acquired silicone properties to fine-tune your end product.

Here's how Silaplane can be used in Alumina-filled dispersion and how it affects the Viscosity

improved viscosity with reactive silicones




Practically, this means two things
  • It lowers the viscosity of dispersion, maintaining the thermal conductivity with the same filler fill ratio

  • It increases the heat dissipation perfromance (thermal conductivity)by further increase of the filler filling ratio

Products for Filler dispersion

Product Structural formula Molecular weight Specific gravity Viscosity
FM-0411P

Hydroxy

1,000 0.96 10 - 25
FM-0421 5,000 0.97 60 - 80
FM-0425 10,000 0.97 140 - 180
FM-DA11 Diol

1,000 0.97 50 - 70
FM-DA21 5,000 0.97 80 - 160
FM-DA26 15,000 0.97 300 - 700

Synthetic Leather Application

PVC-based artificial leather relies on plasticizers such as DOTP (Dioctyl Terephthalate) to achieve softness, flexibility, and long-term durability. However, traditional artificial leather systems often struggle with plasticizer migration, which leads to:

  • Hardening or embrittlement
  • Loss of flexibility
  • Cracking during aging or repeated bending
  • Surface defects caused by heat, oils, solvents, or moisture exposure

To address this challenge, reactive silicones specifically bi-terminal hydroxy-functional PDMS offer a highly effective solution that enhances performance, stability, and longevity.

How Reactive Silicones Prevent DOTP Migration

Bi-terminal PDMS contains reactive hydroxyl groups on both chain ends, allowing it to chemically bond into polyurethane (PU) networks during polymerization. Once incorporated, the PDMS soft segment forms a flexible, low-surface-energy barrier that blocks or significantly reduces DOTP movement.

Network Anchoring Concept


    PU network      PDMS soft block        PU network
---------●-----------( ~~~~~~~ )-----------●---------


(1) The two reactive ends (●) covalently bond into the PU matrix.
(2) The PDMS block becomes structurally locked into the polymer network.
(3) This immobilized PDMS acts as a diffusion shield, preventing DOTP from migrating toward the surface.
(4) Because the silicone is chemically bound, it cannot bleed, volatilize, or carry plasticizer molecules with it.

The result is more stable, durable artificial leather with better retention of softness and flexibility over time.

Compatible Chemistry for PU Leather Systems


Artificial leather producers commonly use a polyol + isocyanate (PU) polymerization system.
This chemistry is fully compatible with hydroxy-functional reactive PDMS.

Reaction Mechanism (Urethane Bond Formation)

HO–PDMS–OH        +        OCN–R–NCO  
(Hydroxy bi-terminal)         (diisocyanate)

Reaction (1) Formation of Urethane Bonds
R–NCO + HO– → R–NH–CO–O–

Resulting Bond Structure:

R–NH–CO–O–PDMS–O–CO–NH–R

This final structure embeds the PDMS chain into the PU backbone, creating a flexible soft segment with excellent migration-blocking properties.

Benefits of Using Reactive PDMS in Artificial Leather

  • Prevents DOTP migration and preserves material softness
  • Improves heat-aging resistance
  • Enhances flexibility and crack resistance
  • Reduces surface damage when exposed to oils, solvents, or moisture
  • Provides a long-lasting silicone effect without bleeding
  • Improves hand-feel and surface smoothness
  • Enhances durability for automotive, upholstery, and footwear applications

Products for Leather Application

Product Structural formula Molecular weight Specific gravity Viscosity
FM-4411 Hydroxy

1,000 0.97 30 - 40
FM-4421 5,000 0.98 100 - 125
FM-4425 15,000 0.97 250 - 400

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers